Ask the water-based paint expert -water-based glass paint appears prickly heat when baking Problem: I use water-based acrylic and amino resin to make the glass paint when baking prickly heat. The details are as follows: Temperature: 80 degrees Time: 2 minutes It was already smooth when it was put into the oven Flash dry for 10 minutes Has been changed to defoamer, leveling agent, solvent, no effec...
How to solve the water - based acrylic paint back adhesion problem? - ask a water-based paint expert Problem: How to solve the water - based acrylic paint back adhesion problem? Water - based acrylic paint back adhesion is a problem often encountered by water - based paint formulators.In order to solve the problem of water - based acrylic paint adhesion, we must fundamentally unders...
Baking performance of water-based glass paint - ask an expert for water-based paint. Question: I would like to ask about the water-based glass baking paint .Water has a boiling point of 100 degrees Celsius, so if you bake it at 140 degrees, it won't boil and bubble up and destroy the film. Right? Response: Water - based paint to balance the evaporation of water and film curing between the relation...
Problem:Some of the materials used in the construction of wood products are plywood and wood chip fiberboard. One of the rubber is the most afraid of water, water paint spray will dissolve the inside of the glue. The effect that USES close lacquer also is not ideal, how should solve? Is it easy to use sinograce chemical raw material solution? thank you . Response:This type of wood is usually ...
Question: Dear expert, I am now eager to develop a new water-based paint mainly for wood. The problem that needs to be solved urgently is the drying time of water-based paint. I want his dry time to be in 30 seconds, can you achieve excuse me, excuse me be colophony its key effect. Response: Hello, the dry time of water - based paint has two concepts commonly."Surface dryness" refers to the basic ...
Question: how to make water-borne heat-resistant paint and water-borne silver powder paint? Whose resin is better? Can you provide the reference formula? Response: Hello, Mr.Zheng,We have received many similar requests for reference formulations.Industrial coatings are characterized by their complexity.It is water borne anti-rust paint likewise,because use environment and the different that ask, f...
Water-based paint sticky sticky brush - Ask a water paint expert Problem:Water-based paint, when brushing, paint is easy to stick to the brush, so that the color is not loose. What is this, please? Answer:the reasons why water-based paint is sticky and sticky are as follows 1.High viscosity of water-based paint: if the viscosity of water-based paint is high, the paint will stick to the brush as yo...
Oil pocket phenomenon in water-based paint Problem: To make furniture with transparent colors, in order to save the craft and achieve the purpose of simple construction. We added water-based Color Concentrate to the topcoat for spraying, and the resulting topcoat contained some oil pockets or other unacceptable "face problems." Reply: Aqueous color concentrates are generally made of metal complexe...
Problem:I have not done waterborne polyurethane, the waterborne paint is a rookie .I have never done water - based, water -based is a rookie,I wonder if waterborne polyurethane also needs curing agent? If you want to use it, what is the ratio?Because of the presence of water, is it possible to go back and consume the curing agent?And I want to use this to make the electroplated silver, is it ok? R...
Is the water-based wood paint film as hard as possible? In the market of waterborne wood lacquers, hardness is one of the most concerned indicators for many Chinese waterborne paint developers and users.In the traditional concept, the harder the paint film, the better. There are often customer consultations for ways to get the paint film to 2H or even 3H.Although waterborne wood lacquers have impr...
Filming aids in waterborne coatings Problem : Why do you need to add filming aids to one-component waterborne coatings? The emulsion alone does not form a film. Filming aids are added to form a film. Why does the film-forming auxiliary volatilize, which is still a complete film, and is different from a film without a filming aid? Why can't a single emulsion be fused by water to produce a capillary...
Wood closed primer formula solves the outstanding problem of wood grain Wood bulges and deforms or wood grain protuberant,It is a common problem in wood painting. We discussed the causes and solutions of this problem in this year's topic.In the article on wood grain protrusions - water-based paints, we recommend three technical solutions: 1. Use a saturated coating of 3-4% binder solids....
Factors Affecting Shrinkage of Waterborne Coating Films In practice, the main causes of shrinkage are as follows: 1. The substrate is contaminated by oil or impurities 2. Apply a paint to the old paint or finish without sanding 3. The interval between constructions of the two paints is too long 4. Too much defoamer in the paint The following focuses on two factors: defoamer and impurity contaminat...
Basic knowledge of water-based paint In order to provide product development support to a wide range of waterborne coating formulation technicians and waterborne coatings sales personnel, we hav collected and summarized a large number of domestic and international market trends and technical points. Visit our waterborne coatings knowledge base and you can see all of our formulation techniques and ...
Classification and characteristics of waterborne coatings - Waterborne acrylic coatings The emulsifier that USES when polymerization can be anionic, also can be nonionic or cationic, corresponding latex and the lacquer that make also can call anionic, nonionic or cationic. Acrylic waterborne wood lacquer is a variety of applications that have been used earlier and are still in large quantities. Si...
Classification and characteristics of water-based coatings - water-based alkyd paints The vegetable oil is reacted with an acid anhydride after alcoholysis to form an alkyd resin, and the content of the hydrophilic group can be increased to form a water-soluble or water-dispersible resin.Water-soluble water-based alkyds are quite transparent in appearance but have color,The alkyd emulsion was brow...