Baking performance of water-based glass paint - ask an expert for water-based paint. Question: I would like to ask about the water-based glass baking paint .Water has a boiling point of 100 degrees Celsius, so if you bake it at 140 degrees, it won't boil and bubble up and destroy the film. Right? Response: Water - based paint to balance the evaporation of water and film curing between the relation...
Leveling and rheological properties of waterborne coatings Problem: water borne white coating wants to have certain rheological already, want to maintain just right leveling sex again, how to do? Response: This problem is one of the characteristics and technical characteristics of water based paint,In principle, it is mainly the relationship between equilibrium viscosity and rheology (plasticity)....
Water-based wood paint runs off oil---Ask a water paint expert Question: Waterborne wood lacquer should run oil to a rainy day only, or brush one day, also can run oil when waiting for the 2nd day to brush again, did especially ugly later . Water-based white paint does not have this problem. The problem ofwater-based varnish is obvious. Answer: Although it is a water-based paint, the film is hydro...
Wood bumps - Common problems with water paint Wood grain is exposed when broken or damaged wood comes into contact with water.A good example of this is when a curved toothpick is placed in water, it will draw water through the capillaries, elongate, and straighten.When the fibers on the board are exposed, they suck water into the wood like a straw, causing the fibers to swell and stick to the surf...
Problem:Some of the materials used in the construction of wood products are plywood and wood chip fiberboard. One of the rubber is the most afraid of water, water paint spray will dissolve the inside of the glue. The effect that USES close lacquer also is not ideal, how should solve? Is it easy to use sinograce chemical raw material solution? thank you . Response:This type of wood is usually ...
Question: Dear expert, I am now eager to develop a new water-based paint mainly for wood. The problem that needs to be solved urgently is the drying time of water-based paint. I want his dry time to be in 30 seconds, can you achieve excuse me, excuse me be colophony its key effect. Response: Hello, the dry time of water - based paint has two concepts commonly."Surface dryness" refers to the basic ...
Question: how to make water-borne heat-resistant paint and water-borne silver powder paint? Whose resin is better? Can you provide the reference formula? Response: Hello, Mr.Zheng,We have received many similar requests for reference formulations.Industrial coatings are characterized by their complexity.It is water borne anti-rust paint likewise,because use environment and the different that ask, f...
Water-based paint sticky sticky brush - Ask a water paint expert Problem:Water-based paint, when brushing, paint is easy to stick to the brush, so that the color is not loose. What is this, please? Answer:the reasons why water-based paint is sticky and sticky are as follows 1.High viscosity of water-based paint: if the viscosity of water-based paint is high, the paint will stick to the brush as yo...
Oil pocket phenomenon in water-based paint Problem: To make furniture with transparent colors, in order to save the craft and achieve the purpose of simple construction. We added water-based Color Concentrate to the topcoat for spraying, and the resulting topcoat contained some oil pockets or other unacceptable "face problems." Reply: Aqueous color concentrates are generally made of metal complexe...
PH adjustment of water-based paint-Ask water character paint expert Question: If the pH value of the water-based paint is not weakly alkaline or the pH value is unstable, what effect will it have in actual use? Thank you! Response: The unstable pH of water-based paints has two main effects on water-based paints.One is that it affects the stability of the filler or paste in the resin because the pH...
Is the water-based wood paint film as hard as possible? In the market of waterborne wood lacquers, hardness is one of the most concerned indicators for many Chinese waterborne paint developers and users.In the traditional concept, the harder the paint film, the better. There are often customer consultations for ways to get the paint film to 2H or even 3H.Although waterborne wood lacquers have impr...
Is the black spot on the surface of the water-based paint mildew? Problem: The wooden doors of our company's surface veneer have no black spots before they are painted. After spraying the water-based paint (primer + top coat), black spots appear on the veneer during the natural drying process. I wonder if the water-based paint is mildewed? If the oil-based colorant is used to seal the bottom, will...
Filming aids in waterborne coatings Problem : Why do you need to add filming aids to one-component waterborne coatings? The emulsion alone does not form a film. Filming aids are added to form a film. Why does the film-forming auxiliary volatilize, which is still a complete film, and is different from a film without a filming aid? Why can't a single emulsion be fused by water to produce a capillary...
The relationship between film formation and MFFT of waterborne coatings This week, Mr. Li asked us three questions through our questioning water-based paint expert column. This is the second problem: Problem: Film formation above MFFT, no film formation below MFFT, what happens during above or below the MFFT, resulting in film formation? Above MFFT, the emulsion particles are soft and hard below. ...
Wood closed primer formula solves the outstanding problem of wood grain Wood bulges and deforms or wood grain protuberant,It is a common problem in wood painting. We discussed the causes and solutions of this problem in this year's topic.In the article on wood grain protrusions - water-based paints, we recommend three technical solutions: 1. Use a saturated coating of 3-4% binder solids....
Formation of shrinkage cavity problems in waterborne coatings The surface defects of the coating film are mainly depressions, pinholes, and the edges or thick edges of the corners. There are two kinds of cases on the surface of the coating film, one is a circular depression, and a hexagonal polygonal depression. The depression on the surface of the coating film is caused by the surface tension gra...