April 12, 2019, the 40-days orange war ended, every partners in this war to pay 100% of the effort, made a different victories,, although the end of the war, but we never give up, the spirit of teamwork will always be maintained, let us move forward.
Common problems of water based paint: causes of shrinkage and solutions Shrinkage, known as cratering, is a common problem with water-based paints。The main cause of shrinkage cavity is impurities in water-based paint. In particular, there is oil in the area where the shrinkage cavity occurs, making the area unable to be wetted.In practical operation, the main causes of shrinkage cavity are as foll...
Waterborne two-component paint seeds and loss of light - ask water-based paint experts Question: Hello! I have two problems with the double-surface water-based topcoat. One is that when the film is thick, it is easy to produce rash [related to defoaming agent or related to water and curing agent to produce CO2?]. One is a double component. After mixing for 2 hours, it will lose light. What is the ...
Formation of shrinkage cavity problems in waterborne coatings The surface defects of the coating film are mainly depressions, pinholes, and the edges or thick edges of the corners. There are two kinds of cases on the surface of the coating film, one is a circular depression, and a hexagonal polygonal depression. The depression on the surface of the coating film is caused by the surface tension gra...
Factors Affecting Shrinkage of Waterborne Coating Films In practice, the main causes of shrinkage are as follows: 1. The substrate is contaminated by oil or impurities 2. Apply a paint to the old paint or finish without sanding 3. The interval between constructions of the two paints is too long 4. Too much defoamer in the paint The following focuses on two factors: defoamer and impurity contaminat...
Abstract: Reducing the shrinkage of water-based paint film is focused on prevention,designing a rational paint formulation,controlling the paint manufacturing process, and strictly controlling the detection of paint materials, which can reduce the chance of shrinkage. Shrinkage holes have been caused, and it is usually difficult to completely solve them. It is necessary to control the degree of sh...
Labelexpo Europe 2019 at the period of 24-27 September, 2019 in BRUSSELS, Belgium At Labelexpo Europe 2019, view hundreds of live demonstrations of the latest innovations, examine the most advanced collection of label and package printing technologies and acquire what your business needs to succeed. Explore the world’s largest label and package printing trade show and advance ten steps ahead of th...
Future development of waterborne paint: In foreign countries, the application of waterborne paint is very wide, especially in the application of home decoration is very mature. In domestic already many enterprises are used at inside ark besmear, cane implement besmear is installed wait With the development of waterborne paint technology, waterborne paint will become a very important paint in furni...
Classification and characteristics of water-based coatings - water-based alkyd paints The vegetable oil is reacted with an acid anhydride after alcoholysis to form an alkyd resin, and the content of the hydrophilic group can be increased to form a water-soluble or water-dispersible resin.Water-soluble water-based alkyds are quite transparent in appearance but have color,The alkyd emulsion was brow...
Water - based coating formulation design system Waterborne coatings, including waterborne wood lacquers, are water-based dispersions and diluents. Unlike conventional solvent-based coatings, the formulation system is a more complex system.When formulating, not only the type of polymer, the properties of the emulsion and the dispersion are concerned. It is also necessary to rationally select variou...
Defoamer is one of the most difficult additives in waterborne wood coatings to control the balance between defoaming and leveling.The paint liquid will generate bubbles during the application due to agitation .If the bubbles present in the paint are not removed in time, the film will dry and form an unacceptable flaw.The paint also produces air bubbles during production, pumping and filling. Defoa...
Character Mineral oil Primer Matte Strong defoaming ability higher price Different product performance differences Large adjustment space Improper selection can cause film defects Influence gloss, flow equality Non-silicone non-oil Various types of coatings, especially in high gloss finishes There are many defoamers on the market, and the choices are very cautious and can be noted in several ways:...
Formulation design system for water based coatings - wetting leveling agent The wetting leveling agent can effectively reduce the surface tension of the system and significantly improve the construction effect of the waterborne wood lacquer.After the addition of the wetting leveling agent, the wetting property and permeability of the paint increase, the leveling property of the paint liquid is imp...
Feature Traditional surfactants (mainly anionic or nonionic) Putty and low-grade system Efficient Reduce static surface tension Good effect on contaminated substrates Easy to cause surface problems Not easy to control High price PSAMS Wide adaptability Common application Minimize possible defects Minimize possible defects Low water sensitivity Low foaming Good dynamic effect expensive visit us sin...
The types and functions of surface control agents include: 1.Improve flow and leveling 2.Reduce friction coefficient and increase slip 3.Enhanced scratch resistance 4.Anti-blocking 5.Enhance the arrangement of matte powder, etc. 6.Special feel, such as softness, etc. 7.Others such as improving the water resistance and stain resistance of the coating film On the one hand, they balance the surface t...
Wood coating process 1.There are many large holes in the hard wood, putty or hole adding agent to flatten; 2.Apply closing primer after hole filling; 3.If you need to deepen the surface texture of the wood and highlight the wood grain, you can apply the closed primer and apply the water color; 4.After conditioning the wood grain, apply two closed primer; 5.Finish with top coat. Sinograce Chemical ...