Oil pocket phenomenon in water-based paint Problem: To make furniture with transparent colors, in order to save the craft and achieve the purpose of simple construction. We added water-based Color Concentrate to the topcoat for spraying, and the resulting topcoat contained some oil pockets or other unacceptable "face problems." Reply: Aqueous color concentrates are generally made of metal complexe...
PH adjustment of water-based paint-Ask water character paint expert Question: If the pH value of the water-based paint is not weakly alkaline or the pH value is unstable, what effect will it have in actual use? Thank you! Response: The unstable pH of water-based paints has two main effects on water-based paints.One is that it affects the stability of the filler or paste in the resin because the pH...
Is the black spot on the surface of the water-based paint mildew? Problem: The wooden doors of our company's surface veneer have no black spots before they are painted. After spraying the water-based paint (primer + top coat), black spots appear on the veneer during the natural drying process. I wonder if the water-based paint is mildewed? If the oil-based colorant is used to seal the bottom, will...
Filming aids in waterborne coatings Problem : Why do you need to add filming aids to one-component waterborne coatings? The emulsion alone does not form a film. Filming aids are added to form a film. Why does the film-forming auxiliary volatilize, which is still a complete film, and is different from a film without a filming aid? Why can't a single emulsion be fused by water to produce a capillary...
Wood closed primer formula solves the outstanding problem of wood grain Wood bulges and deforms or wood grain protuberant,It is a common problem in wood painting. We discussed the causes and solutions of this problem in this year's topic.In the article on wood grain protrusions - water-based paints, we recommend three technical solutions: 1. Use a saturated coating of 3-4% binder solids....
Formation of shrinkage cavity problems in waterborne coatings The surface defects of the coating film are mainly depressions, pinholes, and the edges or thick edges of the corners. There are two kinds of cases on the surface of the coating film, one is a circular depression, and a hexagonal polygonal depression. The depression on the surface of the coating film is caused by the surface tension gra...
Application of water-based paint coating technology The Paint coating With water-based solvent: non-toxic, non-irritating, environmentally friendly, in line with modern people's fashion taste, convenient construction, good flexibility of paint film. Paint dilution and master the viscosity of the construction directly mixed with water. Advantages of water-based paint: One of the most environmentall...
Future development of waterborne paint: In foreign countries, the application of waterborne paint is very wide, especially in the application of home decoration is very mature. In domestic already many enterprises are used at inside ark besmear, cane implement besmear is installed wait With the development of waterborne paint technology, waterborne paint will become a very important paint in furni...
Basic knowledge of water-based paint In order to provide product development support to a wide range of waterborne coating formulation technicians and waterborne coatings sales personnel, we hav collected and summarized a large number of domestic and international market trends and technical points. Visit our waterborne coatings knowledge base and you can see all of our formulation techniques and ...
Classification and characteristics of waterborne coatings - Waterborne acrylic coatings The emulsifier that USES when polymerization can be anionic, also can be nonionic or cationic, corresponding latex and the lacquer that make also can call anionic, nonionic or cationic. Acrylic waterborne wood lacquer is a variety of applications that have been used earlier and are still in large quantities. Si...
Classification and characteristics of waterborne coatings - waterborne polyurethane coatings Polyurethane is a general term for a class of macromolecular compounds having a carbamate structure in a molecular structure, and is usually produced by a polyaddition reaction of a diisocyanate and a polyol. In view of the variety of isocyanates and polyols, the resulting polyurethanes can range from soft...
Classification and characteristics of water-based coatings - water-based alkyd paints The vegetable oil is reacted with an acid anhydride after alcoholysis to form an alkyd resin, and the content of the hydrophilic group can be increased to form a water-soluble or water-dispersible resin.Water-soluble water-based alkyds are quite transparent in appearance but have color,The alkyd emulsion was brow...
Sol-gel coating Classification and characteristics of waterborne coatings - sol /gel coatings Sol-Gel coatings is a new type of coating that has received special attention in recent years. The progress of inorganic nanopowders has promoted the development of sol-gel coatings.The main component of the sol-gel coating is an organic resin and a silane compound, and the silane is hydrolyzed to form a ...
Classification and characteristics of waterborne coatings - waterborne light curing coatings Waterborne light curing coating is a kind of coating classified by curing method. It is a very important kind of coating.In any polymer molecule, a structure in which a reactive group capable of being decomposed by a photoinitiator or a structure capable of being excited by a high-energy radiation to produ...
Formulation design system for waterborne coatings - film forming AIDS The polymer constituting the emulsion or dispersion generally has a glass transition temperature higher than room temperature. In order for the emulsion particles to be well fused into a uniform paint film, it is necessary to reduce the minimum film formation temperature (MFFT) of the crystallization aid.Film form...
Formulation design system for waterborne coatings - film forming AIDS The polymer constituting the emulsion or dispersion generally has a glass transition temperature higher than room temperature. In order for the emulsion particles to be well fused into a uniform paint film, it is necessary to reduce the minimum film formation temperature (MFFT) of the crystallization aid.Film form...