Baking performance of water-based glass paint - ask an expert for water-based paint. Question: I would like to ask about the water-based glass baking paint .Water has a boiling point of 100 degrees Celsius, so if you bake it at 140 degrees, it won't boil and bubble up and destroy the film. Right? Response: Water - based paint to balance the evaporation of water and film curing between the relation...
Wood bumps - Common problems with water paint Wood grain is exposed when broken or damaged wood comes into contact with water.A good example of this is when a curved toothpick is placed in water, it will draw water through the capillaries, elongate, and straighten.When the fibers on the board are exposed, they suck water into the wood like a straw, causing the fibers to swell and stick to the surf...
Problem:I have not done waterborne polyurethane, the waterborne paint is a rookie .I have never done water - based, water -based is a rookie,I wonder if waterborne polyurethane also needs curing agent? If you want to use it, what is the ratio?Because of the presence of water, is it possible to go back and consume the curing agent?And I want to use this to make the electroplated silver, is it ok? R...
Is the water-based wood paint film as hard as possible? In the market of waterborne wood lacquers, hardness is one of the most concerned indicators for many Chinese waterborne paint developers and users.In the traditional concept, the harder the paint film, the better. There are often customer consultations for ways to get the paint film to 2H or even 3H.Although waterborne wood lacquers have impr...
Filming aids in waterborne coatings Problem : Why do you need to add filming aids to one-component waterborne coatings? The emulsion alone does not form a film. Filming aids are added to form a film. Why does the film-forming auxiliary volatilize, which is still a complete film, and is different from a film without a filming aid? Why can't a single emulsion be fused by water to produce a capillary...
The relationship between film formation and MFFT of waterborne coatings This week, Mr. Li asked us three questions through our questioning water-based paint expert column. This is the second problem: Problem: Film formation above MFFT, no film formation below MFFT, what happens during above or below the MFFT, resulting in film formation? Above MFFT, the emulsion particles are soft and hard below. ...
Labelexpo Europe 2019 at the period of 24-27 September, 2019 in BRUSSELS, Belgium At Labelexpo Europe 2019, view hundreds of live demonstrations of the latest innovations, examine the most advanced collection of label and package printing technologies and acquire what your business needs to succeed. Explore the world’s largest label and package printing trade show and advance ten steps ahead of th...
The film-forming aids for waterborne wood coatings are generally alcohol ether type solvents. The most commonly used filming aids such as diethanol ethers, propylene glycol ethers and N-methylpyrrolidone have high and low boiling points.Water-based wood coatings in the summer construction, the water volatilization is faster, that is, the surface is relatively fast, some of the moisture may be encl...
From the viewpoints of molecular structure, molecular polarity and molecular interaction force, the adhesion of the paint film results from the polar group orientation of the polymer molecules in the coating, and its polar group with the polar molecules on the surface of the coated object. The mutual attraction between each other.Only when the polar phase of the two is adapted to obtain a good adh...
Cohesion and thermal expansion coefficient of paint film The force caused by the cohesion of molecules of the same substance is called cohesion.The more cohesive the coating, the worse the adhesion.In the drying process of paint, with the increase of solvent volatilization and crosslinking degree, the cohesion between film forming material molecules increases, the film produces shrinkage phenomeno...
Water - based acrylic emulsion formulation needs to be considered: water - based acrylic resin composition The choice of emulsion raw materials is the most important decision for engineers when formulating aqueous paint formulations.The main properties of the coating are determined by the resin.A wide variety of water-based acrylate emulsions, including polystyrene-acrylate emulsions, are on the m...
What parameters of resin determine coating gloss? Question: What parameters of the resin determine the gloss of the film? Some people say that it is solid content, some people say it is OH value. So, what is the most important determinant of gloss? Answer: There are many parameters that determine the gloss of the paint film. The saturation of the resin: that is, its monomer structure, this index d...
Water based polyurethane resin refers to a binary colloidal system in which a polyurethane resin is dissolved or dispersed in water.Water-based polyurethane resin has the advantages of easy to use, stable performance, strong adhesion, excellent gloss, good heat resistance, etc. It can be suitable for various printing methods, especially suitable for screen printing, plastic packaging and composite...
Development trend of waterborne polyurethane: Nowadays, with the stricter requirements of environmental protection policies, the environmental protection requirements for the performance of adhesives will become higher and higher. Therefore, the greening and environmental protection of composite materials will be more and more important. There will be even more urgency.Therefore, the points mentio...
Precautions for using two-component polyurethane adhesives 1.Before applying the adhesive, the surface of the adherend must be clean, dry and free of grease. 2.The resin and curing agent should be mixed in the required ratio. 3.When scraping the glue, please try to scrape it carefully as it has a defoaming effect. 4.Store adhesive in (> 10, <50 * C) and dry place 5.Run out of the mixed glue ...
Polyurethane and general epoxy products application The use of the two products requires strengthened compressive tensile cement floors or floors and drainage ditches that are resistant to corrosion by strong acids and alkalis, such as chemicals, metallurgical plants, electroplating plants, power plants, pharmaceutical plants, PCB circuit board plants, paper mills, Hardware factory, printing and d...