Categories
new blog
In gravure printing, ink resolubility is also a key indicator to test the performance of ink. Especially in the color ink printing, the moderate resolubility can not only make the color fully displayed, but also solve the problem of shallow plate mesh blocking and overprinting cross-color. In color ink printing, according to the different hue requirements, the depth of the ink hole mesh of the pri...
In order to prevent ink delamination and pigment precipitation, users must be fully stirred before printing. The following summarizes the faults and elimination methods of screen printing ink in use for your reference. 1.Poor adhesion: the reason is improper selection of ink, insufficient pre-press treatment, impurities in the substrate, insufficient drying temperature, insufficient time, improper...
With the development of the application of digital inkjet printing technology in the clothing industry, environmental monitoring is more stringent and the demand for small batch production and personalized customization is increasing. Therefore, the requirements for textile coating ink are becoming higher and higher, and the raw materials for the production of textile coating ink are bec...
What is a peelable resin? Strippable resin is a special resin material with strippable properties (also known as removable film resin). It is often used in the preparation of protective films for electronic products, packaging of semiconductor devices, etc., which can protect these products more intact, and it is easy to peel off when it needs to be replaced or disassembled. When prepari...
Protective film resin Automobile coating resin High resilience waterborne polyurethane resin 1.Typical properties Appearance: Milky white liquid Protective film resin Automobile coating resin Ph: 7.0-9.0 Automobile coating resin Solid content: 40±1% Charge: Anionic High resilience waterborne polyurethane resin Viscosity (25℃): 300-800cP Elongation (%): >200...
As an important material for printing, ink is composed of resin, pigment, filler and auxiliary. Due to many industries such as books, packaging, construction, and circuit boards, with the gradual increase in social demand, the use of ink is also increasing. However, in the production and use of ink, due to the addition of surfactants, equipment stirring operation and environmental changes will cau...
Color paste, also known as pigment paste, is an important form of dye application, which is widely used in textile, ink, paint and other industries. In the classification of pastes, low-halogen pastes and ordinary pastes are two common types. They have certain differences in composition, performance and use, and the differences between the two types of pastes will be discussed in detail below. Fir...
PTFE coatings (polytetrafluoroethylene) are non-stick, fluoropolymer containing high temperature coatings, they have a single coating system or a double coating system of primer and top coat, and have a variety of properties. The Teflon spray process is an important surface treatment that gives objects outstanding properties. With the right preparation, spraying procedures and techniques, Teflon s...
Rubber mold, silicone mold, shoe mold, latex pillow mattress mold, anti-stick easy mold Teflon spray, good model flon coating, non-stick mold surface treatment process The role of mold coating Molds are common tools in the manufacturing industry and are used to make a variety of products. In order to capture the service life and production efficiency of the mold, people often coat the surface of t...
The most important difference between non-stick cookware and ordinary cookware is that the surface is coated with a layer of non-stick paint, and the Teflon non-stick cookware commonly used on the market is to coat the main raw material of fluorinated resin such as polytetrafluoroethylene coating on the metal surface such as aluminum, copper or iron, and through sintering. Properties of NI-PTFE co...
First: the treatment of the substrate First, the substrate (aluminum, stainless steel or other metal substrate) is baked at high temperature (360℃×30 minutes ~380℃×10 minutes) to carbonize the grease or degreaser cleaning for the first step of degreasing. Step 2: Roughening the surface Available corundum sand 80#~120#, pressure 0.4~0.6mpa, sandblasting, so that the surface roughness of the substra...
In the face of different needs of different industries, rollers also need to do the corresponding coating treatment, so as to improve or compensate the relevant performance of the roller. So what are the surface coating technologies for rollers? 01 Coating treatment The coating treatment of the drum includes zinc plating, chromium plating, nickel plating, etc. The different coating treatment can i...
Teflon is the abbreviation of polytetrafluoroethylene, this material has the characteristics of acid and alkali resistance, resistance to various organic solvents, almost insoluble in all solvents, so it has the title of "non-stick coating". With the development of thermal spraying technology, Teflon coatings can be applied to stainless steel, copper, aluminum, magnesium and various alloy metal ma...
Main properties of Teflon coating Teflon high-performance special coating is a fluorine coating based on polytetrafluoroethylene matrix resin, the English name is Teflon, because of the pronunciation, it is usually called Teflon, Teflon, Teflon, Teflon, etc. (all are translations of Teflon). Teflon coatings are a unique, high-performance coating that combines heat resistance, chemical inertia, exc...
Teflon coating is one of the commonly used protective coatings in metal thermal spraying processing technology services, with good non-stick, wear resistance, corrosion resistance, high temperature resistance and other characteristics, can be applied to carbon steel, stainless steel, aluminum, copper, magnesium and various alloys and other metal materials. It can also be applied to non-metall...
Many people think that the temperature of the primer baking (dry) of Teflon paint is not important, just bake it, in fact, this is a misunderstanding. If you usually encounter the following situations, please carefully bake the primer. For the primer coating of Teflon paint, we recommend a temperature of 150 ° C, after the workpiece reaches 150 ° C, bake for 5-10 minutes. I. If the temperature of ...
Copyright © 2015-2025 Anhui Sinograce Chemical Co., Ltd..All Rights Reserved.powered by dyyseo.com