Leveling and rheological properties of waterborne coatings Problem: water borne white coating wants to have certain rheological already, want to maintain just right leveling sex again, how to do? Response: This problem is one of the characteristics and technical characteristics of water based paint,In principle, it is mainly the relationship between equilibrium viscosity and rheology (plasticity)....
Water-based wood paint runs off oil---Ask a water paint expert Question: Waterborne wood lacquer should run oil to a rainy day only, or brush one day, also can run oil when waiting for the 2nd day to brush again, did especially ugly later . Water-based white paint does not have this problem. The problem ofwater-based varnish is obvious. Answer: Although it is a water-based paint, the film is hydro...
April 12, 2019, the 40-days orange war ended, every partners in this war to pay 100% of the effort, made a different victories,, although the end of the war, but we never give up, the spirit of teamwork will always be maintained, let us move forward.
Problem:Some of the materials used in the construction of wood products are plywood and wood chip fiberboard. One of the rubber is the most afraid of water, water paint spray will dissolve the inside of the glue. The effect that USES close lacquer also is not ideal, how should solve? Is it easy to use sinograce chemical raw material solution? thank you . Response:This type of wood is usually ...
Oil pocket phenomenon in water-based paint Problem: To make furniture with transparent colors, in order to save the craft and achieve the purpose of simple construction. We added water-based Color Concentrate to the topcoat for spraying, and the resulting topcoat contained some oil pockets or other unacceptable "face problems." Reply: Aqueous color concentrates are generally made of metal complexe...
Problem:I have not done waterborne polyurethane, the waterborne paint is a rookie .I have never done water - based, water -based is a rookie,I wonder if waterborne polyurethane also needs curing agent? If you want to use it, what is the ratio?Because of the presence of water, is it possible to go back and consume the curing agent?And I want to use this to make the electroplated silver, is it ok? R...
Is the water-based wood paint film as hard as possible? In the market of waterborne wood lacquers, hardness is one of the most concerned indicators for many Chinese waterborne paint developers and users.In the traditional concept, the harder the paint film, the better. There are often customer consultations for ways to get the paint film to 2H or even 3H.Although waterborne wood lacquers have impr...
Filming aids in waterborne coatings Problem : Why do you need to add filming aids to one-component waterborne coatings? The emulsion alone does not form a film. Filming aids are added to form a film. Why does the film-forming auxiliary volatilize, which is still a complete film, and is different from a film without a filming aid? Why can't a single emulsion be fused by water to produce a capillary...
The relationship between film formation and MFFT of waterborne coatings This week, Mr. Li asked us three questions through our questioning water-based paint expert column. This is the second problem: Problem: Film formation above MFFT, no film formation below MFFT, what happens during above or below the MFFT, resulting in film formation? Above MFFT, the emulsion particles are soft and hard below. ...
Formation of shrinkage cavity problems in waterborne coatings The surface defects of the coating film are mainly depressions, pinholes, and the edges or thick edges of the corners. There are two kinds of cases on the surface of the coating film, one is a circular depression, and a hexagonal polygonal depression. The depression on the surface of the coating film is caused by the surface tension gra...
Application of water-based paint coating technology The Paint coating With water-based solvent: non-toxic, non-irritating, environmentally friendly, in line with modern people's fashion taste, convenient construction, good flexibility of paint film. Paint dilution and master the viscosity of the construction directly mixed with water. Advantages of water-based paint: One of the most environmentall...
Basic knowledge of water-based paint In order to provide product development support to a wide range of waterborne coating formulation technicians and waterborne coatings sales personnel, we hav collected and summarized a large number of domestic and international market trends and technical points. Visit our waterborne coatings knowledge base and you can see all of our formulation techniques and ...
Classification and characteristics of waterborne coatings - waterborne polyurethane coatings Polyurethane is a general term for a class of macromolecular compounds having a carbamate structure in a molecular structure, and is usually produced by a polyaddition reaction of a diisocyanate and a polyol. In view of the variety of isocyanates and polyols, the resulting polyurethanes can range from soft...
Sol-gel coating Classification and characteristics of waterborne coatings - sol /gel coatings Sol-Gel coatings is a new type of coating that has received special attention in recent years. The progress of inorganic nanopowders has promoted the development of sol-gel coatings.The main component of the sol-gel coating is an organic resin and a silane compound, and the silane is hydrolyzed to form a ...
In the formulation of waterborne wood lacquer topcoats, the binder is a key component in forming the film and determining the properties of the film. The binder, ie the polymer emulsion, dispersion or hybrid, accounts for more than 80%, preferably more than 90%.Since the solid content of the emulsion, especially the aqueous dispersion is relatively low (the aqueous dispersion is generally 30% to 3...
Formulation design system for waterborne coatings - film forming AIDS The polymer constituting the emulsion or dispersion generally has a glass transition temperature higher than room temperature. In order for the emulsion particles to be well fused into a uniform paint film, it is necessary to reduce the minimum film formation temperature (MFFT) of the crystallization aid.Film form...