Waterborne wood lacquer grain display is not clear enough
- 2020-02-29 16:54:24
- admin
Asked by water-based paint experts: water-based wood lacquer wood grain display is not clear enough Question: Our company is now doing the first coat of wood lacquer and tried a water-based resin (polyurethane). and there is no problem with the adhesion.The current problem is that after adding color essence, it is applied to the floor and the wood grain display is not clear enough. The amount of t...
-
Water-based paint knowledge base-water-based glass paint appears prickly heat when baking
- 2020-02-29 16:03:18
- admin
Ask the water-based paint expert -water-based glass paint appears prickly heat when baking Problem: I use water-based acrylic and amino resin to make the glass paint when baking prickly heat. The details are as follows: Temperature: 80 degrees Time: 2 minutes It was already smooth when it was put into the oven Flash dry for 10 minutes Has been changed to defoamer, leveling agent, solvent, no effec...
-
How to solve the water - based acrylic paint back adhesion problem
- 2020-02-29 15:15:06
- admin
How to solve the water - based acrylic paint back adhesion problem? - ask a water-based paint expert Problem: How to solve the water - based acrylic paint back adhesion problem? Water - based acrylic paint back adhesion is a problem often encountered by water - based paint formulators.In order to solve the problem of water - based acrylic paint adhesion, we must fundamentally unders...
-
Baking performance of water-based glass paint
- 2020-02-29 15:06:29
- admin
Baking performance of water-based glass paint - ask an expert for water-based paint. Question: I would like to ask about the water-based glass baking paint .Water has a boiling point of 100 degrees Celsius, so if you bake it at 140 degrees, it won't boil and bubble up and destroy the film. Right? Response: Water - based paint to balance the evaporation of water and film curing between the relation...
-
Water-based paint knowledge base-Wood bumps
- 2020-02-29 14:20:25
- admin
Wood bumps - Common problems with water paint Wood grain is exposed when broken or damaged wood comes into contact with water.A good example of this is when a curved toothpick is placed in water, it will draw water through the capillaries, elongate, and straighten.When the fibers on the board are exposed, they suck water into the wood like a straw, causing the fibers to swell and stick to the surf...
-
Is the water based wood paint film as hard as possible
- 2020-02-24 08:44:38
- admin
Is the water-based wood paint film as hard as possible? In the market of waterborne wood lacquers, hardness is one of the most concerned indicators for many Chinese waterborne paint developers and users.In the traditional concept, the harder the paint film, the better. There are often customer consultations for ways to get the paint film to 2H or even 3H.Although waterborne wood lacquers have impr...
-
The relationship between film formation and MFFT of waterborne coatings
- 2020-02-22 17:44:24
- admin
The relationship between film formation and MFFT of waterborne coatings This week, Mr. Li asked us three questions through our questioning water-based paint expert column. This is the second problem: Problem: Film formation above MFFT, no film formation below MFFT, what happens during above or below the MFFT, resulting in film formation? Above MFFT, the emulsion particles are soft and hard below. ...
-
Formulation design system for waterborne coatings - film forming AIDS 2
- 2020-02-22 10:09:29
- admin
The film-forming aids for waterborne wood coatings are generally alcohol ether type solvents. The most commonly used filming aids such as diethanol ethers, propylene glycol ethers and N-methylpyrrolidone have high and low boiling points.Water-based wood coatings in the summer construction, the water volatilization is faster, that is, the surface is relatively fast, some of the moisture may be encl...
-
Polarity of paint film and painted surface
- 2020-02-21 13:39:38
- admin
From the viewpoints of molecular structure, molecular polarity and molecular interaction force, the adhesion of the paint film results from the polar group orientation of the polymer molecules in the coating, and its polar group with the polar molecules on the surface of the coated object. The mutual attraction between each other.Only when the polar phase of the two is adapted to obtain a good adh...
-
Cohesion and thermal expansion coefficient of paint film
- 2020-02-21 13:35:17
- admin
Cohesion and thermal expansion coefficient of paint film The force caused by the cohesion of molecules of the same substance is called cohesion.The more cohesive the coating, the worse the adhesion.In the drying process of paint, with the increase of solvent volatilization and crosslinking degree, the cohesion between film forming material molecules increases, the film produces shrinkage phenomeno...
-
Water - based acrylic emulsion formulation needs to be considered: water - based acrylic resin composition
- 2020-02-21 10:51:07
- admin
Water - based acrylic emulsion formulation needs to be considered: water - based acrylic resin composition The choice of emulsion raw materials is the most important decision for engineers when formulating aqueous paint formulations.The main properties of the coating are determined by the resin.A wide variety of water-based acrylate emulsions, including polystyrene-acrylate emulsions, are on the m...
-
Factors that determine the gloss of the coating
- 2020-02-20 22:28:22
- admin
What parameters of resin determine coating gloss? Question: What parameters of the resin determine the gloss of the film? Some people say that it is solid content, some people say it is OH value. So, what is the most important determinant of gloss? Answer: There are many parameters that determine the gloss of the paint film. The saturation of the resin: that is, its monomer structure, this index d...
-
2.Substrate treatment - one of the waterborne wood coating process series
- 2020-02-20 22:09:52
- admin
The third step in the treatment of water-based paint coated substrates is sealing. The role of the water-based putty is to make the surface of the substrate such as wood not very regular and smooth and minor defects and defects, such as pores, fine cracks, pits, joints and concrete, to reduce the surface roughness and increase the flatness.The requirements for water-based putty are good adhesion a...
-
What is water-based polyurethane resin
- 2020-02-20 18:19:56
- admin
Water based polyurethane resin refers to a binary colloidal system in which a polyurethane resin is dissolved or dispersed in water.Water-based polyurethane resin has the advantages of easy to use, stable performance, strong adhesion, excellent gloss, good heat resistance, etc. It can be suitable for various printing methods, especially suitable for screen printing, plastic packaging and composite...
-
Development trend of waterborne polyurethane:
- 2020-02-20 17:47:56
- admin
Development trend of waterborne polyurethane: Nowadays, with the stricter requirements of environmental protection policies, the environmental protection requirements for the performance of adhesives will become higher and higher. Therefore, the greening and environmental protection of composite materials will be more and more important. There will be even more urgency.Therefore, the points mentio...
-
Precautions for using two-component polyurethane adhesives
- 2020-02-20 17:27:05
- admin
Precautions for using two-component polyurethane adhesives 1.Before applying the adhesive, the surface of the adherend must be clean, dry and free of grease. 2.The resin and curing agent should be mixed in the required ratio. 3.When scraping the glue, please try to scrape it carefully as it has a defoaming effect. 4.Store adhesive in (> 10, <50 * C) and dry place 5.Run out of the mixed glue ...