Water-based paint sticky sticky brush - Ask a water paint expert Problem:Water-based paint, when brushing, paint is easy to stick to the brush, so that the color is not loose. What is this, please? Answer:the reasons why water-based paint is sticky and sticky are as follows 1.High viscosity of water-based paint: if the viscosity of water-based paint is high, the paint will stick to the brush as yo...
Problem:I have not done waterborne polyurethane, the waterborne paint is a rookie .I have never done water - based, water -based is a rookie,I wonder if waterborne polyurethane also needs curing agent? If you want to use it, what is the ratio?Because of the presence of water, is it possible to go back and consume the curing agent?And I want to use this to make the electroplated silver, is it ok? R...
Is the water-based wood paint film as hard as possible? In the market of waterborne wood lacquers, hardness is one of the most concerned indicators for many Chinese waterborne paint developers and users.In the traditional concept, the harder the paint film, the better. There are often customer consultations for ways to get the paint film to 2H or even 3H.Although waterborne wood lacquers have impr...
Filming aids in waterborne coatings Problem : Why do you need to add filming aids to one-component waterborne coatings? The emulsion alone does not form a film. Filming aids are added to form a film. Why does the film-forming auxiliary volatilize, which is still a complete film, and is different from a film without a filming aid? Why can't a single emulsion be fused by water to produce a capillary...
The relationship between film formation and MFFT of waterborne coatings This week, Mr. Li asked us three questions through our questioning water-based paint expert column. This is the second problem: Problem: Film formation above MFFT, no film formation below MFFT, what happens during above or below the MFFT, resulting in film formation? Above MFFT, the emulsion particles are soft and hard below. ...
Wood closed primer formula solves the outstanding problem of wood grain Wood bulges and deforms or wood grain protuberant,It is a common problem in wood painting. We discussed the causes and solutions of this problem in this year's topic.In the article on wood grain protrusions - water-based paints, we recommend three technical solutions: 1. Use a saturated coating of 3-4% binder solids....
Factors Affecting Shrinkage of Waterborne Coating Films In practice, the main causes of shrinkage are as follows: 1. The substrate is contaminated by oil or impurities 2. Apply a paint to the old paint or finish without sanding 3. The interval between constructions of the two paints is too long 4. Too much defoamer in the paint The following focuses on two factors: defoamer and impurity contaminat...
Future development of waterborne paint: In foreign countries, the application of waterborne paint is very wide, especially in the application of home decoration is very mature. In domestic already many enterprises are used at inside ark besmear, cane implement besmear is installed wait With the development of waterborne paint technology, waterborne paint will become a very important paint in furni...
Basic knowledge of water-based paint In order to provide product development support to a wide range of waterborne coating formulation technicians and waterborne coatings sales personnel, we hav collected and summarized a large number of domestic and international market trends and technical points. Visit our waterborne coatings knowledge base and you can see all of our formulation techniques and ...
Classification and characteristics of waterborne coatings - Waterborne acrylic coatings The emulsifier that USES when polymerization can be anionic, also can be nonionic or cationic, corresponding latex and the lacquer that make also can call anionic, nonionic or cationic. Acrylic waterborne wood lacquer is a variety of applications that have been used earlier and are still in large quantities. Si...
Classification and characteristics of water-based coatings - water-based alkyd paints The vegetable oil is reacted with an acid anhydride after alcoholysis to form an alkyd resin, and the content of the hydrophilic group can be increased to form a water-soluble or water-dispersible resin.Water-soluble water-based alkyds are quite transparent in appearance but have color,The alkyd emulsion was brow...
In the formulation of waterborne wood lacquer topcoats, the binder is a key component in forming the film and determining the properties of the film. The binder, ie the polymer emulsion, dispersion or hybrid, accounts for more than 80%, preferably more than 90%.Since the solid content of the emulsion, especially the aqueous dispersion is relatively low (the aqueous dispersion is generally 30% to 3...
The film-forming aids for waterborne wood coatings are generally alcohol ether type solvents. The most commonly used filming aids such as diethanol ethers, propylene glycol ethers and N-methylpyrrolidone have high and low boiling points.Water-based wood coatings in the summer construction, the water volatilization is faster, that is, the surface is relatively fast, some of the moisture may be encl...
Defoamer is one of the most difficult additives in waterborne wood coatings to control the balance between defoaming and leveling.The paint liquid will generate bubbles during the application due to agitation .If the bubbles present in the paint are not removed in time, the film will dry and form an unacceptable flaw.The paint also produces air bubbles during production, pumping and filling. Defoa...
Water - based coating formulation design system - matting agent Matting agents are additives used to control the gloss of waterborne wood coatings to meet the broad needs of mainstream matt paints in today's market.The extinction mechanism of the matting agent can be arranged in an orderly manner on the surface of the coating film, so that the surface of the coating film is uneven, causing the lig...
Waterborne paint formulation design system - pH regulator Waterborne wood coatings may also need to adjust the pH when necessary.Most emulsions or aqueous dispersions have been adjusted to a pH of 8 to 9 when they are produced, eliminating the need for pH adjusters when making paint.If the pH value is different, add 0.05% to 0.1% of the pH adjuster during the paint making process, and adjust the p...