How to solve the poor adhesion of water-based paint after soaking in water?
Problems: water-based acrylic resin, self-drying system,60 ℃ / 120 minutes after the bubble row down into the water, can use fingernail.But after taking out to wait
for water to be able again, how should solve?
Response:
This test method is still very harsh.General water - based resins, acrylic acid, polyurethane or Self-crosslinking single component system, are difficult to
meet.Consider the following alternatives:
1.Avoid resin systems with common surfactants.
2.If the resin system contains carboxyl group, why consider adding zinc salt to increase the crosslinking degree?
3. You can also consider adding some wax emulsion to increase the hydrophobicity of the formula.
Sinograce Chemical produces acrylic emulsion, acrylic resin,water based polyurethane resin , wood paint, water based industrial paint, water based building glue and other water based coatings.
visit us sinograce chemical: https://www.sinogracechem.com
Get a Quote Now :sales@sinogracechem.com
Telephone :+86 0551 63459511
sinograce chemical
Sinograce Chemical is professional technical enterprise providing solutions of surface materials and manufacturing of raw materials. Sinograce Chemical Company is composed of R&D center, Manufacture center, Quality control department, Market center and International trade department. We have been dedicating to research on excellent paint/coating, adhesive for over 15 years. And now still conti...
Room 1013, Building A5, Financial Port Center, Yangzijiang Road, Baohe District, Hefei City, Anhui province, China
+86 0551 63459511
Copyright © 2015-2025 Anhui Sinograce Chemical Co., Ltd..All Rights Reserved.powered by dyyseo.com
top