1.The cause of a back adhesion:
(1)the paste itself anti-viscosity, especially in the wet weather easy to stick back;
(2)After the printing is completed, it is packaged without perfect heat treatment;
(3)adjust the slurry formula is not appropriate, adding too much transparent slurry easy to cause back adhesion;
(4)transport or storage conditions are not good, in high temperature, high humidity conditions for a long time stack.
Treatment methods for back adhesion:
(1)choose good anti - sticky paste printing;
2.Reasons for poor elasticity:
(1)The selection of sizing technology and printing fabric do not match;
(2)After printing drying treatment is not complete;
(3)too much crosslinking agent will affect the size of the elasticity and softness.
(4)add excessive destruction of resin tensile material (urea, ammonia).
3.Causes of color transfer phenomenon:
(1)when mixing the selection of color species poor resistance to migration;(4)transport or storage conditions are not good, in high temperature, high humidity conditions for a long time stack.
Treatment of color transfer phenomenon:
(1)selection of good color species resistant to migration to adjust the paste.(3)In transportation and storage, as far as possible flat, do not fold together or with insulation paper.
Sinograce Chemical produces water-based polymers for PE, BOPP and other film water-based inks,
visit us sinograce chemical: https://www.sinogracechem.com
Get a Quote Now :sales@sinogracechem.com
Telephone :+86 0551 63459511
Copyright © 2015-2025 Anhui Sinograce Chemical Co., Ltd..All Rights Reserved.powered by dyyseo.com
top