Question: how to make water-borne heat-resistant paint and water-borne silver powder paint? Whose resin is better? Can you provide the reference formula? Response: Hello, Mr.Zheng,We have received many similar requests for reference formulations.Industrial coatings are characterized by their complexity.It is water borne anti-rust paint likewise,because use environment and the different that ask, f...
Oil pocket phenomenon in water-based paint Problem: To make furniture with transparent colors, in order to save the craft and achieve the purpose of simple construction. We added water-based Color Concentrate to the topcoat for spraying, and the resulting topcoat contained some oil pockets or other unacceptable "face problems." Reply: Aqueous color concentrates are generally made of metal complexe...
Is the water-based wood paint film as hard as possible? In the market of waterborne wood lacquers, hardness is one of the most concerned indicators for many Chinese waterborne paint developers and users.In the traditional concept, the harder the paint film, the better. There are often customer consultations for ways to get the paint film to 2H or even 3H.Although waterborne wood lacquers have impr...
Filming aids in waterborne coatings Problem : Why do you need to add filming aids to one-component waterborne coatings? The emulsion alone does not form a film. Filming aids are added to form a film. Why does the film-forming auxiliary volatilize, which is still a complete film, and is different from a film without a filming aid? Why can't a single emulsion be fused by water to produce a capillary...
Factors Affecting Shrinkage of Waterborne Coating Films In practice, the main causes of shrinkage are as follows: 1. The substrate is contaminated by oil or impurities 2. Apply a paint to the old paint or finish without sanding 3. The interval between constructions of the two paints is too long 4. Too much defoamer in the paint The following focuses on two factors: defoamer and impurity contaminat...
In the formulation of waterborne wood lacquer topcoats, the binder is a key component in forming the film and determining the properties of the film. The binder, ie the polymer emulsion, dispersion or hybrid, accounts for more than 80%, preferably more than 90%.Since the solid content of the emulsion, especially the aqueous dispersion is relatively low (the aqueous dispersion is generally 30% to 3...
Formulation design system for waterborne coatings - film forming AIDS The polymer constituting the emulsion or dispersion generally has a glass transition temperature higher than room temperature. In order for the emulsion particles to be well fused into a uniform paint film, it is necessary to reduce the minimum film formation temperature (MFFT) of the crystallization aid.Film form...
Formulation design system for waterborne coatings - film forming AIDS The polymer constituting the emulsion or dispersion generally has a glass transition temperature higher than room temperature. In order for the emulsion particles to be well fused into a uniform paint film, it is necessary to reduce the minimum film formation temperature (MFFT) of the crystallization aid.Film form...
Formulation design system for waterborne coatings - film forming AIDS The polymer constituting the emulsion or dispersion generally has a glass transition temperature higher than room temperature. In order for the emulsion particles to be well fused into a uniform paint film, it is necessary to reduce the minimum film formation temperature (MFFT) of the crystallization aid.Film forming agents are ...
The types and functions of surface control agents include: 1.Improve flow and leveling 2.Reduce friction coefficient and increase slip 3.Enhanced scratch resistance 4.Anti-blocking 5.Enhance the arrangement of matte powder, etc. 6.Special feel, such as softness, etc. 7.Others such as improving the water resistance and stain resistance of the coating film On the one hand, they balance the surface t...
Water - based coating formulation design system - matting agent Matting agents are additives used to control the gloss of waterborne wood coatings to meet the broad needs of mainstream matt paints in today's market.The extinction mechanism of the matting agent can be arranged in an orderly manner on the surface of the coating film, so that the surface of the coating film is uneven, causing the lig...
Wood coating process 1.There are many large holes in the hard wood, putty or hole adding agent to flatten; 2.Apply closing primer after hole filling; 3.If you need to deepen the surface texture of the wood and highlight the wood grain, you can apply the closed primer and apply the water color; 4.After conditioning the wood grain, apply two closed primer; 5.Finish with top coat. Sinograce Chemical ...
Water - based acrylic emulsion formulation needs to be considered: water - based acrylic resin composition The choice of emulsion raw materials is the most important decision for engineers when formulating aqueous paint formulations.The main properties of the coating are determined by the resin.A wide variety of water-based acrylate emulsions, including polystyrene-acrylate emulsions, are on the m...
The internal structure of waterborne acrylic emulsion particles will affect several aspects of waterborne paint formulations.According to the order in which the effects are affected, the phase structure will first affect the selection and addition of the filming aid.Different phases have different hydrophilic/lipophilic characteristics, and the oleophilic properties of various coalescents are diff...
What parameters of resin determine coating gloss? Question: What parameters of the resin determine the gloss of the film? Some people say that it is solid content, some people say it is OH value. So, what is the most important determinant of gloss? Answer: There are many parameters that determine the gloss of the paint film. The saturation of the resin: that is, its monomer structure, this index d...
1.The cause of a back adhesion: (1)the paste itself anti-viscosity, especially in the wet weather easy to stick back; (2)After the printing is completed, it is packaged without perfect heat treatment; (3)adjust the slurry formula is not appropriate, adding too much transparent slurry easy to cause back adhesion; (4)transport or storage conditions are not good, in high temperature, high humidity co...