1.The cause of a back adhesion: 
	(1)the paste itself anti-viscosity, especially in the wet weather easy to stick back; 
	(2)After the printing is completed, it is packaged without perfect heat treatment; 
	(3)adjust the slurry formula is not appropriate, adding too much transparent slurry easy to cause back adhesion; 
(4)transport or storage conditions are not good, in high temperature, high humidity conditions for a long time stack.
	
	Treatment methods for back adhesion: 
(1)choose good anti - sticky paste printing;
(2)Good heat treatment for printing products;
(3)Pay attention to the mixing formula, if the transparent pulp more than 80% is easy to cause back adhesion, so you can add an appropriate amount of curing agent or anti-adhesion agent for treatment;
(4)Please pay attention to the improvement of transportation and storage conditions.
(5)with anti - stick items to strengthen the whole processing.
	
 
	2.Reasons for poor elasticity: 
	(1)The selection of sizing technology and printing fabric do not match; 
	(2)After printing drying treatment is not complete; 
	(3)too much crosslinking agent will affect the size of the elasticity and softness. 
	(4)add excessive destruction of resin tensile material (urea, ammonia). 
	
 
	3.Causes of color transfer phenomenon: 
(1)when mixing the selection of color species poor resistance to migration;
(2)add excessive color species;
(3)printing products dry processing;
	(4)transport or storage conditions are not good, in high temperature, high humidity conditions for a long time stack. 
	
 
	Treatment of color transfer phenomenon: 
(1)selection of good color species resistant to migration to adjust the paste.
(2)Good heat treatment for printing products;
(3)In transportation and storage, as far as possible flat, do not fold together or with insulation paper.
3.Causes of color transfer phenomenon:
(1)when mixing the selection of color species poor resistance to migration;
(2)add excessive color species;
(3)printing products dry processing;
(4)transport or storage conditions are not good, in high temperature, high humidity conditions for a long time stack.
Treatment of color transfer phenomenon:
(1)selection of good color species resistant to migration to adjust the paste.
(2)Good heat treatment for printing products;
	(3)In transportation and storage, as far as possible flat, do not fold together or with insulation paper. 
	  
	Sinograce Chemical produces water-based polymers for PE, BOPP and other film water-based inks,
 
	 
	visit us sinograce chemical: https://www.sinogracechem.com 
	Get a Quote Now :sales@sinogracechem.com 
	Telephone               :+86 0551 63459511