A research report of market research firm Reportlinker recently released show that the global wood resin market will reach $4 billion 240 million by 2021, a CAGR of 5.39%. With the growing demand for environmental protection coating and the implementation of the VOC regulations, water-based coating resin and solventless resin market develop, in addition, the downstream industry demand in the next ...
According to the relevant research report released "2020 global waterborne epoxy resin market trend and forecast (according to the application ((coatings, composites, adhesives and other industries )), terminal (automotive, construction, textile, furniture, packaging etc.)) and regional division)" carried out the analysis and forecast of market scale of water epoxy resin. Global water based epoxy ...
August 21, 2017,Anhui sinograce Chemical Co., Ltd held an event launching ceremony of “2017 Orange War” in Hefei Big Shu mountain. The purpose of this activity is not only to thank each employee through thick and thin with the company in the first half of 2017 and their hard to pay, but also providing a stage for the staff to full show themselves. Increase interaction in activities, prom...
In the formulation of water-based coatings, the selection of raw materials is the most important decision.The main performance of the coating is determined by resin.Water-based acrylate emulsion,including polystyrene acrylate emulsion,a great variety and market jumbly. Different water-based acrylic resin composition have a great impact on the film-forming and cost of water-based coatings. 1.Princi...
The internal structure of the aqueous acrylic emulsion particles will have an impact on several aspects of the water-based paint formulation. the phase structure will first affect the choice and addition of film forming auxiliaries.Different phases have different hydrophilic / lipophilic characteristics,the lipophilicity of film forming additives is also different.For example, two propyl...
Anhui SINOGRACE chemical on September 30, 2017, Company employees to visit Shangchuan Island for two days, Came to the beauty of the fishing port, We appreciate the sunset and sunrise, The first taste of wild pineapple, Swimming in the seaside, Looking for a lovely hermit crab on the shore, Follow the fisherman fishing, When the sun was setting, we eat dinner at the seaside. Thank t...
Water-based wood paint resin is the main raw material for the production of water-based wood paint. It can be used as varnish, paint the bottom dual-use resin. It is widely used in water-based industrial wood coatings, water-based decoration coatings and other fields. Water-based wood paint resin is divided into water-based wood paint and oily wood paint. Oily paint consists of organic solvents. I...
With the progress of water-based resin technology, water-based paint technology has been recognized by more and more industries and applications. In promoting environmental protection at the same time, water-based paint its special hydrophilic structure may also lead to premature failure of the coating. We usually attribute the cause of failure to resin performance defects, while ignoring the wate...
Water - based wood paint common problems: gloss wood paint uneven luster Phenomenon There is light coating on the wood surface, coating film gloss, some areas of low gloss. Cause The wood fiber and pith ray in cork are loose with the growth of growth rings, the base material infiltrates excessively, the coating film increases the pigment volume concentration due to the decrease of the base ma...
How to solve the poor adhesion of water-based paint after soaking in water? Problems: water-based acrylic resin, self-drying system,60 ℃ / 120 minutes after the bubble row down into the water, can use fingernail.But after taking out to wait for water to be able again, how should solve? Response: This test method is still very harsh.General water - based resins, acrylic acid, polyurethane or Self-c...
Asked by water-based paint experts: water-based wood lacquer wood grain display is not clear enough Question: Our company is now doing the first coat of wood lacquer and tried a water-based resin (polyurethane). and there is no problem with the adhesion.The current problem is that after adding color essence, it is applied to the floor and the wood grain display is not clear enough. The amount of t...
Ask the water-based paint expert -water-based glass paint appears prickly heat when baking Problem: I use water-based acrylic and amino resin to make the glass paint when baking prickly heat. The details are as follows: Temperature: 80 degrees Time: 2 minutes It was already smooth when it was put into the oven Flash dry for 10 minutes Has been changed to defoamer, leveling agent, solvent, no effec...
How to solve the water - based acrylic paint back adhesion problem? - ask a water-based paint expert Problem: How to solve the water - based acrylic paint back adhesion problem? Water - based acrylic paint back adhesion is a problem often encountered by water - based paint formulators.In order to solve the problem of water - based acrylic paint adhesion, we must fundamentally unders...
Baking performance of water-based glass paint - ask an expert for water-based paint. Question: I would like to ask about the water-based glass baking paint .Water has a boiling point of 100 degrees Celsius, so if you bake it at 140 degrees, it won't boil and bubble up and destroy the film. Right? Response: Water - based paint to balance the evaporation of water and film curing between the relation...
Wood bumps - Common problems with water paint Wood grain is exposed when broken or damaged wood comes into contact with water.A good example of this is when a curved toothpick is placed in water, it will draw water through the capillaries, elongate, and straighten.When the fibers on the board are exposed, they suck water into the wood like a straw, causing the fibers to swell and stick to the surf...
Is the water-based wood paint film as hard as possible? In the market of waterborne wood lacquers, hardness is one of the most concerned indicators for many Chinese waterborne paint developers and users.In the traditional concept, the harder the paint film, the better. There are often customer consultations for ways to get the paint film to 2H or even 3H.Although waterborne wood lacquers have impr...