Categories
new blog
How to solve the poor adhesion of water-based paint after soaking in water? Problems: water-based acrylic resin, self-drying system,60 ℃ / 120 minutes after the bubble row down into the water, can use fingernail.But after taking out to wait for water to be able again, how should solve? Response: This test method is still very harsh.General water - based resins, acrylic acid, polyurethane or Self-c...
Case study of water-based paint: the quality of water-based paint is unstable Maintaining the stability of waterborne coatings is one of the keys to the success of waterborne coatings manufacturers. This is especially important for manufacturers of industrial waterborne paints. There are many reasons for the unstable quality of water based paint, such as water-based paint process,water-based paint...
Asked by water-based paint experts: water-based wood lacquer wood grain display is not clear enough Question: Our company is now doing the first coat of wood lacquer and tried a water-based resin (polyurethane). and there is no problem with the adhesion.The current problem is that after adding color essence, it is applied to the floor and the wood grain display is not clear enough. The amount of t...
Asked by water-based paint experts: water-based paints appear flocculated in the production process Problem: Our company produced a batch of waterborne paint last week. The formula remains unchanged. After the completion of production, the coating appears a mass flocculent,it is difficult to remove the filtration, the quality of waterborne coating is reduced. What is the cause? What method c...
Ask the water-based paint expert -water-based glass paint appears prickly heat when baking Problem: I use water-based acrylic and amino resin to make the glass paint when baking prickly heat. The details are as follows: Temperature: 80 degrees Time: 2 minutes It was already smooth when it was put into the oven Flash dry for 10 minutes Has been changed to defoamer, leveling agent, solvent, no effec...
How to solve the water - based acrylic paint back adhesion problem? - ask a water-based paint expert Problem: How to solve the water - based acrylic paint back adhesion problem? Water - based acrylic paint back adhesion is a problem often encountered by water - based paint formulators.In order to solve the problem of water - based acrylic paint adhesion, we must fundamentally unders...
Baking performance of water-based glass paint - ask an expert for water-based paint. Question: I would like to ask about the water-based glass baking paint .Water has a boiling point of 100 degrees Celsius, so if you bake it at 140 degrees, it won't boil and bubble up and destroy the film. Right? Response: Water - based paint to balance the evaporation of water and film curing between the relation...
Leveling and rheological properties of waterborne coatings Problem: water borne white coating wants to have certain rheological already, want to maintain just right leveling sex again, how to do? Response: This problem is one of the characteristics and technical characteristics of water based paint,In principle, it is mainly the relationship between equilibrium viscosity and rheology (plasticity)....
Wood bumps - Common problems with water paint Wood grain is exposed when broken or damaged wood comes into contact with water.A good example of this is when a curved toothpick is placed in water, it will draw water through the capillaries, elongate, and straighten.When the fibers on the board are exposed, they suck water into the wood like a straw, causing the fibers to swell and stick to the surf...
April 12, 2019, the 40-days orange war ended, every partners in this war to pay 100% of the effort, made a different victories,, although the end of the war, but we never give up, the spirit of teamwork will always be maintained, let us move forward.
Problem:Some of the materials used in the construction of wood products are plywood and wood chip fiberboard. One of the rubber is the most afraid of water, water paint spray will dissolve the inside of the glue. The effect that USES close lacquer also is not ideal, how should solve? Is it easy to use sinograce chemical raw material solution? thank you . Response:This type of wood is usually ...
Question: Dear expert, I am now eager to develop a new water-based paint mainly for wood. The problem that needs to be solved urgently is the drying time of water-based paint. I want his dry time to be in 30 seconds, can you achieve excuse me, excuse me be colophony its key effect. Response: Hello, the dry time of water - based paint has two concepts commonly."Surface dryness" refers to the basic ...
Question: how to make water-borne heat-resistant paint and water-borne silver powder paint? Whose resin is better? Can you provide the reference formula? Response: Hello, Mr.Zheng,We have received many similar requests for reference formulations.Industrial coatings are characterized by their complexity.It is water borne anti-rust paint likewise,because use environment and the different that ask, f...
Oil pocket phenomenon in water-based paint Problem: To make furniture with transparent colors, in order to save the craft and achieve the purpose of simple construction. We added water-based Color Concentrate to the topcoat for spraying, and the resulting topcoat contained some oil pockets or other unacceptable "face problems." Reply: Aqueous color concentrates are generally made of metal complexe...
Problem:I have not done waterborne polyurethane, the waterborne paint is a rookie .I have never done water - based, water -based is a rookie,I wonder if waterborne polyurethane also needs curing agent? If you want to use it, what is the ratio?Because of the presence of water, is it possible to go back and consume the curing agent?And I want to use this to make the electroplated silver, is it ok? R...
Is the water-based wood paint film as hard as possible? In the market of waterborne wood lacquers, hardness is one of the most concerned indicators for many Chinese waterborne paint developers and users.In the traditional concept, the harder the paint film, the better. There are often customer consultations for ways to get the paint film to 2H or even 3H.Although waterborne wood lacquers have impr...