Water-in-water multi-color paint spray guns to use most of the spray, for the operation, but also because of the improper use of the gun caused by uneven distribution of the coating,the following together to see how to solve it. The smaller the gun distance, the greater the pressure of the spray, the greater the impact of the product by the pressure of the water, water-in-watercolorful paint coati...
water-based resin | water-based industrial coating (a) water paint common problems Common problems with water-based lacquer wood paint: transparency, Color fullness of shade The complaint that often hears about paint of ability in water is paint of ability in water diapure is poor, cannot show the plump godliness of woodiness. In general, the transparency of water-based paint is determined by the ...
Phenomenon : Part of the water-based paint film from the primer uplift, which contains gas or liquid, showed uneven distribution. Cause 1.When the water-based paint is applied, the dry water-based paint film is exposed to rain. 2.Apply a water-based paint primer to the wet substrate. 3.Water - based paint film is affected by acid - base and heat. Amelioration 1.Considering the gas phase conditions...
Phenomenon: Wood coating water - based varnish after the grain fuzzy, grain color and luster differ, failed to retain the original style of wood. cause 1.Transparent putty transparency is poor or scraping too thick, reduce the clarity of wood grain. 2.Water-based paint storage time is too long, pigment precipitation, on the shallow under the deep operation without mixing evenly, coating film thick...
Common problem of lacquer of waterborne woodwork: varnish besmear film is not level off, burnish is not even Phenomenon : Wood is filled with putty hole processing, after sealing the bottom, coating brush varnish, coating film flatness is low, luster is not uniform. Cause : Hole putty poor quality, loose, solvent absorption. The wood fiber and pith ray on the wood surface are relatively loose. The...
Water - based wood paint common problems: gloss wood paint uneven luster Phenomenon There is light coating on the wood surface, coating film gloss, some areas of low gloss. Cause The wood fiber and pith ray in cork are loose with the growth of growth rings, the base material infiltrates excessively, the coating film increases the pigment volume concentration due to the decrease of the base ma...
How to solve the poor adhesion of water-based paint after soaking in water? Problems: water-based acrylic resin, self-drying system,60 ℃ / 120 minutes after the bubble row down into the water, can use fingernail.But after taking out to wait for water to be able again, how should solve? Response: This test method is still very harsh.General water - based resins, acrylic acid, polyurethane or Self-c...
Case study of water-based paint: the quality of water-based paint is unstable Maintaining the stability of waterborne coatings is one of the keys to the success of waterborne coatings manufacturers. This is especially important for manufacturers of industrial waterborne paints. There are many reasons for the unstable quality of water based paint, such as water-based paint process,water-based paint...
Asked by water-based paint experts: water-based wood lacquer wood grain display is not clear enough Question: Our company is now doing the first coat of wood lacquer and tried a water-based resin (polyurethane). and there is no problem with the adhesion.The current problem is that after adding color essence, it is applied to the floor and the wood grain display is not clear enough. The amount of t...
Asked by water-based paint experts: water-based paints appear flocculated in the production process Problem: Our company produced a batch of waterborne paint last week. The formula remains unchanged. After the completion of production, the coating appears a mass flocculent,it is difficult to remove the filtration, the quality of waterborne coating is reduced. What is the cause? What method c...
Water paint common problems: water paint viscosity deviation index The formulation and process of water based paint remain unchanged. However, the viscosity of the water based paint produced deviates from the index and is not within the control scope, for three reasons: 1.Water based paint raw material properties change. Changes such as filler particle size distribution, oil absorption volatile oi...
How to solve the water - based acrylic paint back adhesion problem? - ask a water-based paint expert Problem: How to solve the water - based acrylic paint back adhesion problem? Water - based acrylic paint back adhesion is a problem often encountered by water - based paint formulators.In order to solve the problem of water - based acrylic paint adhesion, we must fundamentally unders...
April 12, 2019, the 40-days orange war ended, every partners in this war to pay 100% of the effort, made a different victories,, although the end of the war, but we never give up, the spirit of teamwork will always be maintained, let us move forward.
Problem:Some of the materials used in the construction of wood products are plywood and wood chip fiberboard. One of the rubber is the most afraid of water, water paint spray will dissolve the inside of the glue. The effect that USES close lacquer also is not ideal, how should solve? Is it easy to use sinograce chemical raw material solution? thank you . Response:This type of wood is usually ...
Question: how to make water-borne heat-resistant paint and water-borne silver powder paint? Whose resin is better? Can you provide the reference formula? Response: Hello, Mr.Zheng,We have received many similar requests for reference formulations.Industrial coatings are characterized by their complexity.It is water borne anti-rust paint likewise,because use environment and the different that ask, f...
Water-based paint sticky sticky brush - Ask a water paint expert Problem:Water-based paint, when brushing, paint is easy to stick to the brush, so that the color is not loose. What is this, please? Answer:the reasons why water-based paint is sticky and sticky are as follows 1.High viscosity of water-based paint: if the viscosity of water-based paint is high, the paint will stick to the brush as yo...
Copyright © 2015-2025 Anhui Sinograce Chemical Co., Ltd..All Rights Reserved.powered by dyyseo.com