Categories
water-based resin | water-based industrial coating (a) water paint common problems Water based paint common problem: bubble - big bubble Large bubbles are large, visible bubbles that are visible to the naked eye. Bulk bubbles generally occur during the production or application of water-based paints. Possible solutions: 1. Use appropriate defoaming agents In the process of producing water-based pa...
water-based resin | water-based industrial coating (a) water paint common problems Water - based paint common problems: bubble - microbubble Microbubbles are tiny bubbles. If there are microbubbles in the varnish layer, this will reduce the "warmness" of the wood.Each microbubble appears to be a small curved lens that reflects and refracts light, summing up, resulting in a yellow and red color red...
Phenomenon : Part of the water-based paint film from the primer uplift, which contains gas or liquid, showed uneven distribution. Cause 1.When the water-based paint is applied, the dry water-based paint film is exposed to rain. 2.Apply a water-based paint primer to the wet substrate. 3.Water - based paint film is affected by acid - base and heat. Amelioration 1.Considering the gas phase conditions...
Phenomenon: Wood coating water - based varnish after the grain fuzzy, grain color and luster differ, failed to retain the original style of wood. cause 1.Transparent putty transparency is poor or scraping too thick, reduce the clarity of wood grain. 2.Water-based paint storage time is too long, pigment precipitation, on the shallow under the deep operation without mixing evenly, coating film thick...
Common problem of lacquer of waterborne woodwork: varnish besmear film is not level off, burnish is not even Phenomenon : Wood is filled with putty hole processing, after sealing the bottom, coating brush varnish, coating film flatness is low, luster is not uniform. Cause : Hole putty poor quality, loose, solvent absorption. The wood fiber and pith ray on the wood surface are relatively loose. The...
SINOGRACE Chemical has more than 8 years history in exporting chemicals to India. Due to the stable quality and considerate service, the chemicals supplied by SINOGRACE receive good comments locally. Now SINOGRACE is a famous and popular chemical brand in India.
Ask the water-based paint expert -water-based glass paint appears prickly heat when baking Problem: I use water-based acrylic and amino resin to make the glass paint when baking prickly heat. The details are as follows: Temperature: 80 degrees Time: 2 minutes It was already smooth when it was put into the oven Flash dry for 10 minutes Has been changed to defoamer, leveling agent, solvent, no effec...
Water-based wood paint runs off oil---Ask a water paint expert Question: Waterborne wood lacquer should run oil to a rainy day only, or brush one day, also can run oil when waiting for the 2nd day to brush again, did especially ugly later . Water-based white paint does not have this problem. The problem ofwater-based varnish is obvious. Answer: Although it is a water-based paint, the film is hydro...
April 12, 2019, the 40-days orange war ended, every partners in this war to pay 100% of the effort, made a different victories,, although the end of the war, but we never give up, the spirit of teamwork will always be maintained, let us move forward.
Common problems of water based paint: causes of shrinkage and solutions Shrinkage, known as cratering, is a common problem with water-based paints。The main cause of shrinkage cavity is impurities in water-based paint. In particular, there is oil in the area where the shrinkage cavity occurs, making the area unable to be wetted.In practical operation, the main causes of shrinkage cavity are as foll...
Filming aids in waterborne coatings Problem : Why do you need to add filming aids to one-component waterborne coatings? The emulsion alone does not form a film. Filming aids are added to form a film. Why does the film-forming auxiliary volatilize, which is still a complete film, and is different from a film without a filming aid? Why can't a single emulsion be fused by water to produce a capillary...
Waterborne two-component paint seeds and loss of light - ask water-based paint experts Question: Hello! I have two problems with the double-surface water-based topcoat. One is that when the film is thick, it is easy to produce rash [related to defoaming agent or related to water and curing agent to produce CO2?]. One is a double component. After mixing for 2 hours, it will lose light. What is the ...
The relationship between film formation and MFFT of waterborne coatings This week, Mr. Li asked us three questions through our questioning water-based paint expert column. This is the second problem: Problem: Film formation above MFFT, no film formation below MFFT, what happens during above or below the MFFT, resulting in film formation? Above MFFT, the emulsion particles are soft and hard below. ...
Abstract: Reducing the shrinkage of water-based paint film is focused on prevention,designing a rational paint formulation,controlling the paint manufacturing process, and strictly controlling the detection of paint materials, which can reduce the chance of shrinkage. Shrinkage holes have been caused, and it is usually difficult to completely solve them. It is necessary to control the degree of sh...
Labelexpo Europe 2019 at the period of 24-27 September, 2019 in BRUSSELS, Belgium At Labelexpo Europe 2019, view hundreds of live demonstrations of the latest innovations, examine the most advanced collection of label and package printing technologies and acquire what your business needs to succeed. Explore the world’s largest label and package printing trade show and advance ten steps ahead of th...
Future development of waterborne paint: In foreign countries, the application of waterborne paint is very wide, especially in the application of home decoration is very mature. In domestic already many enterprises are used at inside ark besmear, cane implement besmear is installed wait With the development of waterborne paint technology, waterborne paint will become a very important paint in furni...