Water-in-water multi-color paint spray guns to use most of the spray, for the operation, but also because of the improper use of the gun caused by uneven distribution of the coating,the following together to see how to solve it. The smaller the gun distance, the greater the pressure of the spray, the greater the impact of the product by the pressure of the water, water-in-watercolorful paint coati...
Phenomenon : Part of the water-based paint film from the primer uplift, which contains gas or liquid, showed uneven distribution. Cause 1.When the water-based paint is applied, the dry water-based paint film is exposed to rain. 2.Apply a water-based paint primer to the wet substrate. 3.Water - based paint film is affected by acid - base and heat. Amelioration 1.Considering the gas phase conditions...
Water - based wood paint common problems: gloss wood paint uneven luster Phenomenon There is light coating on the wood surface, coating film gloss, some areas of low gloss. Cause The wood fiber and pith ray in cork are loose with the growth of growth rings, the base material infiltrates excessively, the coating film increases the pigment volume concentration due to the decrease of the base ma...
How to solve the poor adhesion of water-based paint after soaking in water? Problems: water-based acrylic resin, self-drying system,60 ℃ / 120 minutes after the bubble row down into the water, can use fingernail.But after taking out to wait for water to be able again, how should solve? Response: This test method is still very harsh.General water - based resins, acrylic acid, polyurethane or Self-c...
Case study of water-based paint: the quality of water-based paint is unstable Maintaining the stability of waterborne coatings is one of the keys to the success of waterborne coatings manufacturers. This is especially important for manufacturers of industrial waterborne paints. There are many reasons for the unstable quality of water based paint, such as water-based paint process,water-based paint...
Asked by water-based paint experts: water-based wood lacquer wood grain display is not clear enough Question: Our company is now doing the first coat of wood lacquer and tried a water-based resin (polyurethane). and there is no problem with the adhesion.The current problem is that after adding color essence, it is applied to the floor and the wood grain display is not clear enough. The amount of t...
Ask the water-based paint expert -water-based glass paint appears prickly heat when baking Problem: I use water-based acrylic and amino resin to make the glass paint when baking prickly heat. The details are as follows: Temperature: 80 degrees Time: 2 minutes It was already smooth when it was put into the oven Flash dry for 10 minutes Has been changed to defoamer, leveling agent, solvent, no effec...
How to solve the water - based acrylic paint back adhesion problem? - ask a water-based paint expert Problem: How to solve the water - based acrylic paint back adhesion problem? Water - based acrylic paint back adhesion is a problem often encountered by water - based paint formulators.In order to solve the problem of water - based acrylic paint adhesion, we must fundamentally unders...
Baking performance of water-based glass paint - ask an expert for water-based paint. Question: I would like to ask about the water-based glass baking paint .Water has a boiling point of 100 degrees Celsius, so if you bake it at 140 degrees, it won't boil and bubble up and destroy the film. Right? Response: Water - based paint to balance the evaporation of water and film curing between the relation...
Wood bumps - Common problems with water paint Wood grain is exposed when broken or damaged wood comes into contact with water.A good example of this is when a curved toothpick is placed in water, it will draw water through the capillaries, elongate, and straighten.When the fibers on the board are exposed, they suck water into the wood like a straw, causing the fibers to swell and stick to the surf...
Question: how to make water-borne heat-resistant paint and water-borne silver powder paint? Whose resin is better? Can you provide the reference formula? Response: Hello, Mr.Zheng,We have received many similar requests for reference formulations.Industrial coatings are characterized by their complexity.It is water borne anti-rust paint likewise,because use environment and the different that ask, f...
Oil pocket phenomenon in water-based paint Problem: To make furniture with transparent colors, in order to save the craft and achieve the purpose of simple construction. We added water-based Color Concentrate to the topcoat for spraying, and the resulting topcoat contained some oil pockets or other unacceptable "face problems." Reply: Aqueous color concentrates are generally made of metal complexe...
Is the water-based wood paint film as hard as possible? In the market of waterborne wood lacquers, hardness is one of the most concerned indicators for many Chinese waterborne paint developers and users.In the traditional concept, the harder the paint film, the better. There are often customer consultations for ways to get the paint film to 2H or even 3H.Although waterborne wood lacquers have impr...
Filming aids in waterborne coatings Problem : Why do you need to add filming aids to one-component waterborne coatings? The emulsion alone does not form a film. Filming aids are added to form a film. Why does the film-forming auxiliary volatilize, which is still a complete film, and is different from a film without a filming aid? Why can't a single emulsion be fused by water to produce a capillary...
The relationship between film formation and MFFT of waterborne coatings This week, Mr. Li asked us three questions through our questioning water-based paint expert column. This is the second problem: Problem: Film formation above MFFT, no film formation below MFFT, what happens during above or below the MFFT, resulting in film formation? Above MFFT, the emulsion particles are soft and hard below. ...
Factors Affecting Shrinkage of Waterborne Coating Films In practice, the main causes of shrinkage are as follows: 1. The substrate is contaminated by oil or impurities 2. Apply a paint to the old paint or finish without sanding 3. The interval between constructions of the two paints is too long 4. Too much defoamer in the paint The following focuses on two factors: defoamer and impurity contaminat...