The method to determine whether the quality of the seal printing tape is poor: Ordinary sealing tape glue is acrylic glue, also known as pressure-sensitive adhesive, the main component is tincture. Tincture is a kind of macromolecular active substance. The activity will be affected by the level of temperature. Tincture content of glue will directly affect the use of tape. Some individuals thi...
Factors affecting the curing speed are the main types of paint, coating thickness, curing methods, curing conditions, curing equipment and specific curing procedures. 1.The type of paint Under the same curing conditions, the type of paint is different, the curing speed is very different. Generally speaking, the volatile paint curing fast, oily paint curing is slow. Polymeric paint is very dif...
Classification and quality requirements of BOPP sealing tape (including ordinary sealing tape, printing tape, high-viscosity antifreeze tape):The series of products mainly to polypropylene film, special polypropylene film, acrylic and water-based acrylic plastic as raw materials and has the characteristics of posting smooth. It is suitable for general packaging and fixed and packaging an...
Sinograce Chemical holds the 2018 employee games at the cultural and sports activities center on July 2, 2018.More than 80 people from six teams took part in the competition. It consists of three events: tug-of-war, table tennis and badminton. In the competition, each team elaborately arranged, strives for success, on the field fully displays each special strength and the ball skill.Off the f...
Colorful paint is mainly used in imitation stone effect, so also known as liquid stone and the horizon exterior paint.is composed of incompatible two-phase components, one of the dispersion medium for the continuous phase, the other phase for the dispersed phase. Painting, through a one-time spray, you can get luxury, beautiful, colorful patterns. The pattern formed by the one-time spraying is com...
Water-in-water multi-color paint spray guns to use most of the spray, for the operation, but also because of the improper use of the gun caused by uneven distribution of the coating,the following together to see how to solve it. The smaller the gun distance, the greater the pressure of the spray, the greater the impact of the product by the pressure of the water, water-in-watercolorful paint coati...
Phenomenon : Part of the water-based paint film from the primer uplift, which contains gas or liquid, showed uneven distribution. Cause 1.When the water-based paint is applied, the dry water-based paint film is exposed to rain. 2.Apply a water-based paint primer to the wet substrate. 3.Water - based paint film is affected by acid - base and heat. Amelioration 1.Considering the gas phase conditions...
Water - based wood paint common problems: gloss wood paint uneven luster Phenomenon There is light coating on the wood surface, coating film gloss, some areas of low gloss. Cause The wood fiber and pith ray in cork are loose with the growth of growth rings, the base material infiltrates excessively, the coating film increases the pigment volume concentration due to the decrease of the base ma...
How to solve the poor adhesion of water-based paint after soaking in water? Problems: water-based acrylic resin, self-drying system,60 ℃ / 120 minutes after the bubble row down into the water, can use fingernail.But after taking out to wait for water to be able again, how should solve? Response: This test method is still very harsh.General water - based resins, acrylic acid, polyurethane or Self-c...
Common problems with water-based paint: oil slick surface of paint Problem: The finished product has floating black spots or impurities on the surface. A lot of coating produce technical personnel to had encountered similar problem, there is in coating production process "small bubble" or small black dot cannot eliminate. Carefully examine these "little bubbles" ~ they are actually small black oil...
Ask the water-based paint expert -water-based glass paint appears prickly heat when baking Problem: I use water-based acrylic and amino resin to make the glass paint when baking prickly heat. The details are as follows: Temperature: 80 degrees Time: 2 minutes It was already smooth when it was put into the oven Flash dry for 10 minutes Has been changed to defoamer, leveling agent, solvent, no effec...
How to solve the water - based acrylic paint back adhesion problem? - ask a water-based paint expert Problem: How to solve the water - based acrylic paint back adhesion problem? Water - based acrylic paint back adhesion is a problem often encountered by water - based paint formulators.In order to solve the problem of water - based acrylic paint adhesion, we must fundamentally unders...
Problem:Some of the materials used in the construction of wood products are plywood and wood chip fiberboard. One of the rubber is the most afraid of water, water paint spray will dissolve the inside of the glue. The effect that USES close lacquer also is not ideal, how should solve? Is it easy to use sinograce chemical raw material solution? thank you . Response:This type of wood is usually ...
Question: Dear expert, I am now eager to develop a new water-based paint mainly for wood. The problem that needs to be solved urgently is the drying time of water-based paint. I want his dry time to be in 30 seconds, can you achieve excuse me, excuse me be colophony its key effect. Response: Hello, the dry time of water - based paint has two concepts commonly."Surface dryness" refers to the basic ...
Question: how to make water-borne heat-resistant paint and water-borne silver powder paint? Whose resin is better? Can you provide the reference formula? Response: Hello, Mr.Zheng,We have received many similar requests for reference formulations.Industrial coatings are characterized by their complexity.It is water borne anti-rust paint likewise,because use environment and the different that ask, f...
Water-based paint sticky sticky brush - Ask a water paint expert Problem:Water-based paint, when brushing, paint is easy to stick to the brush, so that the color is not loose. What is this, please? Answer:the reasons why water-based paint is sticky and sticky are as follows 1.High viscosity of water-based paint: if the viscosity of water-based paint is high, the paint will stick to the brush as yo...