Categories
new blog
In addition to China, the United States, Europe, Japan are the main origin of water-based pressure-sensitive adhesive. Although the world's water-based pressure-sensitive adhesive production cannot be counted,probably the trend can be seen. In the water-based pressure-sensitive adhesive products,transparent sealing tape, stickers label dominant. Production of Pressure-sensitive is low,return ...
With the gradual improvement of national living standards, people on the printing and packaging of exquisite, green and other requirements are getting higher and higher, thus driving the printing and packaging industry to flourish, but also led to a large number of productions about adhesive which is used for printing. One of the water-based adhesive with its water-based environmental protect...
Textile dyeing and finishing auxiliaries according to the production process can be divided into two major categories of textile auxiliaries and printing auxiliaries. Dyeing and finishing auxiliaries in the dyeing and finishing industry is widely used, has penetrated into the printing and dyeing processing of all corners, its main uses are: lubrication, wetting, penetration, promote dyei...
Classification and quality requirements of BOPP sealing tape (including ordinary sealing tape, printing tape, high-viscosity antifreeze tape):The series of products mainly to polypropylene film, special polypropylene film, acrylic and water-based acrylic plastic as raw materials and has the characteristics of posting smooth. It is suitable for general packaging and fixed and packaging an...
2018.6.22,customers from Canada have come to visit our company. Foreign trade manager and relevant personnel warmly welcome our customers, and introduced our product which they are interested in detailedly. The peelable coating is designed using water based polyurethane that can be applied to smooth, non-porous surfaces and simply peeled off once dry. All peelable coatings may be applied with wate...
The exterior wall stone paint of the building is really natural, after the paint is dry,it is like a real stone, and the colors are warm and natural, and the color is fresh and nice. Perhaps a lot of friends, for this anti-stone coating is not very understanding, so,will inevitably feel very strange, then this material really have these advantages? In fact, this anti-stone coating not only has the...
water-based resin | water-based industrial coating (a) water paint common problems Water based paint common problem: bubble - big bubble Large bubbles are large, visible bubbles that are visible to the naked eye. Bulk bubbles generally occur during the production or application of water-based paints. Possible solutions: 1. Use appropriate defoaming agents In the process of producing water-based pa...
water-based resin | water-based industrial coating (a) water paint common problems Water - based paint common problems: bubble - microbubble Microbubbles are tiny bubbles. If there are microbubbles in the varnish layer, this will reduce the "warmness" of the wood.Each microbubble appears to be a small curved lens that reflects and refracts light, summing up, resulting in a yellow and red color red...
Phenomenon : Part of the water-based paint film from the primer uplift, which contains gas or liquid, showed uneven distribution. Cause 1.When the water-based paint is applied, the dry water-based paint film is exposed to rain. 2.Apply a water-based paint primer to the wet substrate. 3.Water - based paint film is affected by acid - base and heat. Amelioration 1.Considering the gas phase conditions...
Phenomenon: Wood coating water - based varnish after the grain fuzzy, grain color and luster differ, failed to retain the original style of wood. cause 1.Transparent putty transparency is poor or scraping too thick, reduce the clarity of wood grain. 2.Water-based paint storage time is too long, pigment precipitation, on the shallow under the deep operation without mixing evenly, coating film thick...
Common problem of lacquer of waterborne woodwork: varnish besmear film is not level off, burnish is not even Phenomenon : Wood is filled with putty hole processing, after sealing the bottom, coating brush varnish, coating film flatness is low, luster is not uniform. Cause : Hole putty poor quality, loose, solvent absorption. The wood fiber and pith ray on the wood surface are relatively loose. The...
Ask the water-based paint expert -water-based glass paint appears prickly heat when baking Problem: I use water-based acrylic and amino resin to make the glass paint when baking prickly heat. The details are as follows: Temperature: 80 degrees Time: 2 minutes It was already smooth when it was put into the oven Flash dry for 10 minutes Has been changed to defoamer, leveling agent, solvent, no effec...
Baking performance of water-based glass paint - ask an expert for water-based paint. Question: I would like to ask about the water-based glass baking paint .Water has a boiling point of 100 degrees Celsius, so if you bake it at 140 degrees, it won't boil and bubble up and destroy the film. Right? Response: Water - based paint to balance the evaporation of water and film curing between the relation...
Water-based wood paint runs off oil---Ask a water paint expert Question: Waterborne wood lacquer should run oil to a rainy day only, or brush one day, also can run oil when waiting for the 2nd day to brush again, did especially ugly later . Water-based white paint does not have this problem. The problem ofwater-based varnish is obvious. Answer: Although it is a water-based paint, the film is hydro...
Common problems of water based paint: causes of shrinkage and solutions Shrinkage, known as cratering, is a common problem with water-based paints。The main cause of shrinkage cavity is impurities in water-based paint. In particular, there is oil in the area where the shrinkage cavity occurs, making the area unable to be wetted.In practical operation, the main causes of shrinkage cavity are as foll...
Waterborne two-component paint seeds and loss of light - ask water-based paint experts Question: Hello! I have two problems with the double-surface water-based topcoat. One is that when the film is thick, it is easy to produce rash [related to defoaming agent or related to water and curing agent to produce CO2?]. One is a double component. After mixing for 2 hours, it will lose light. What is the ...
Copyright © 2015-2025 Anhui Sinograce Chemical Co., Ltd..All Rights Reserved.powered by dyyseo.com
top