Categories
new blog
1.Energy conservation: Water in water multicolor coating, pure water-based formula, excellent raw material technology.Granite stone, depending on nature, the development of powerful resources have some damage to the ecological. Water covered with colorful paint to solve this problem, and decorative curtain wall color can be artificially controlled, energy saving and environmental protection,commen...
water-based resin | water-based industrial coating (a) water paint common problems Water based paint common problem: bubble - big bubble Large bubbles are large, visible bubbles that are visible to the naked eye. Bulk bubbles generally occur during the production or application of water-based paints. Possible solutions: 1. Use appropriate defoaming agents In the process of producing water-based pa...
Phenomenon : Part of the water-based paint film from the primer uplift, which contains gas or liquid, showed uneven distribution. Cause 1.When the water-based paint is applied, the dry water-based paint film is exposed to rain. 2.Apply a water-based paint primer to the wet substrate. 3.Water - based paint film is affected by acid - base and heat. Amelioration 1.Considering the gas phase conditions...
Phenomenon: Wood coating water - based varnish after the grain fuzzy, grain color and luster differ, failed to retain the original style of wood. cause 1.Transparent putty transparency is poor or scraping too thick, reduce the clarity of wood grain. 2.Water-based paint storage time is too long, pigment precipitation, on the shallow under the deep operation without mixing evenly, coating film thick...
Common problem of lacquer of waterborne woodwork: varnish besmear film is not level off, burnish is not even Phenomenon : Wood is filled with putty hole processing, after sealing the bottom, coating brush varnish, coating film flatness is low, luster is not uniform. Cause : Hole putty poor quality, loose, solvent absorption. The wood fiber and pith ray on the wood surface are relatively loose. The...
Water - based wood paint common problems: gloss wood paint uneven luster Phenomenon There is light coating on the wood surface, coating film gloss, some areas of low gloss. Cause The wood fiber and pith ray in cork are loose with the growth of growth rings, the base material infiltrates excessively, the coating film increases the pigment volume concentration due to the decrease of the base ma...
How to solve the poor adhesion of water-based paint after soaking in water? Problems: water-based acrylic resin, self-drying system,60 ℃ / 120 minutes after the bubble row down into the water, can use fingernail.But after taking out to wait for water to be able again, how should solve? Response: This test method is still very harsh.General water - based resins, acrylic acid, polyurethane or Self-c...
Case study of water-based paint: the quality of water-based paint is unstable Maintaining the stability of waterborne coatings is one of the keys to the success of waterborne coatings manufacturers. This is especially important for manufacturers of industrial waterborne paints. There are many reasons for the unstable quality of water based paint, such as water-based paint process,water-based paint...
Asked by water-based paint experts: water-based wood lacquer wood grain display is not clear enough Question: Our company is now doing the first coat of wood lacquer and tried a water-based resin (polyurethane). and there is no problem with the adhesion.The current problem is that after adding color essence, it is applied to the floor and the wood grain display is not clear enough. The amount of t...
Water paint common problems: water paint viscosity deviation index The formulation and process of water based paint remain unchanged. However, the viscosity of the water based paint produced deviates from the index and is not within the control scope, for three reasons: 1.Water based paint raw material properties change. Changes such as filler particle size distribution, oil absorption volatile oi...
Ask the water-based paint expert -water-based glass paint appears prickly heat when baking Problem: I use water-based acrylic and amino resin to make the glass paint when baking prickly heat. The details are as follows: Temperature: 80 degrees Time: 2 minutes It was already smooth when it was put into the oven Flash dry for 10 minutes Has been changed to defoamer, leveling agent, solvent, no effec...
How to solve the water - based acrylic paint back adhesion problem? - ask a water-based paint expert Problem: How to solve the water - based acrylic paint back adhesion problem? Water - based acrylic paint back adhesion is a problem often encountered by water - based paint formulators.In order to solve the problem of water - based acrylic paint adhesion, we must fundamentally unders...
Baking performance of water-based glass paint - ask an expert for water-based paint. Question: I would like to ask about the water-based glass baking paint .Water has a boiling point of 100 degrees Celsius, so if you bake it at 140 degrees, it won't boil and bubble up and destroy the film. Right? Response: Water - based paint to balance the evaporation of water and film curing between the relation...
Leveling and rheological properties of waterborne coatings Problem: water borne white coating wants to have certain rheological already, want to maintain just right leveling sex again, how to do? Response: This problem is one of the characteristics and technical characteristics of water based paint,In principle, it is mainly the relationship between equilibrium viscosity and rheology (plasticity)....
Water-based wood paint runs off oil---Ask a water paint expert Question: Waterborne wood lacquer should run oil to a rainy day only, or brush one day, also can run oil when waiting for the 2nd day to brush again, did especially ugly later . Water-based white paint does not have this problem. The problem ofwater-based varnish is obvious. Answer: Although it is a water-based paint, the film is hydro...
Wood bumps - Common problems with water paint Wood grain is exposed when broken or damaged wood comes into contact with water.A good example of this is when a curved toothpick is placed in water, it will draw water through the capillaries, elongate, and straighten.When the fibers on the board are exposed, they suck water into the wood like a straw, causing the fibers to swell and stick to the surf...